Slagging Agent Deslagging Agent Composite Flux Aluminium Auxiliary Material for Aluminium Casting
1. Using Method
1). Used inside furnace:
when aluminium is melt and heated up to casting temperature, spread slagging agent with shovel onto the slag face, then strike with steel rake lightly, mix aluminium slag for 3-5 minutes, then skim the slag finally.
2). Used outside furnace:
spread slagging agent on aluminium slag removed just a moment ago, and then stir the slag.
2. Use Level: 1.0 - 3.0/T