Refining Agent Degreaser for Aluminium Casting
1. Using Method
Add refining agent of required amount into refining tank and cover it properly, turn on the switch of refining tank and connect nitrogen gas. When refining agent is spraying out of refining iron tube, insert it into the furnace and move all around inside evenly for 2 or 3 times. When powder inside the tank is sprayed completely, draw out the refining tube out of aluminium liquid and then switch off nitrogen gas.
2. Refining Temperature: 700~740℃
3. Refining Time: 8~15 minutes (6~20 ton furnace)